ABSTRACT:
An article of manufacture having improved high temperature oxidation and corrosion resistance comprising: (a) a superalloy substrate containing a carbide reinforcing phase, and (b) a coating consisting of chromium, aluminum, carbon, at least one element selected from iron, cobalt or nickel, and optionally an element selected from yttrium or the rare earth elements.
REFERENCES:
patent: 3573963 (1971-04-01), Maxwell
patent: 3741791 (1973-06-01), Maxwell et al.
patent: 3873347 (1975-03-01), Walker et al.
patent: 4003765 (1977-01-01), Davidson
Jackson Melvin R.
Rairden, III John R.
Cohen Joseph T.
General Electric Company
Kendall Ralph S.
Turner F. Wesley
Watts Charles T.
LandOfFree
Oxidation corrosion resistant superalloys and coatings does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Oxidation corrosion resistant superalloys and coatings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Oxidation corrosion resistant superalloys and coatings will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2090641