ABSTRACT:
Improved coating compositions are described for the protection of superalloys at elevated temperatures. The coatings are of the MCrAlY type where M is nickel or cobalt and are significantly improved by the addition of from 0.1-7% silicon and 0.1-2% hafnium. Coatings of the invention are preferably applied by plasma spraying and as so applied are found to be substantially more effective than prior art coatings.
REFERENCES:
patent: 4034142 (1977-07-01), Hecht
patent: 4054723 (1977-10-01), Higginbotham et al.
patent: 4094673 (1978-06-01), Erickson et al.
patent: 4109061 (1978-08-01), Beale et al.
patent: 4123595 (1978-10-01), Chang
Duvall David S.
Gupta Dinesh K.
Sohl Charles E.
United Technologies Corporation
Yarbrough Amelia B.
LandOfFree
Overlays coating for superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Overlays coating for superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Overlays coating for superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-139822