ABSTRACT:
Improved coating compositions are described for the protection of superalloys at elevated temperatures. The coatings are of the MCrAlY type where M is nickel or cobalt and are significantly improved by the addition of from 0.1-7% silicon and 0.1-2% hafnium. Coatings of the invention are preferably applied by plasma spraying and as so applied are found to be substantially more effective than prior art coatings.

REFERENCES:
patent: 4034142 (1977-07-01), Hecht
patent: 4054723 (1977-10-01), Higginbotham et al.
patent: 4078922 (1978-03-01), Magyar et al.
patent: 4094673 (1978-06-01), Erickson et al.
patent: 4109061 (1978-08-01), Beale et al.
patent: 4123595 (1978-10-01), Chang
patent: 4326011 (1982-04-01), Goebel et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Overlay coatings for superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Overlay coatings for superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Overlay coatings for superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1908157

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.