ABSTRACT:
Prepare an oriented polymer composition that is cavitated, has cross sectional dimensions all at least three millimeters and at least one de-oriented surface layer having a thickness of at least 80 microns and at least 50 microns less than half the thickness of the oriented polymer composition, the de-oriented surface layer having a lower degree of polymer orientation than a 100 micron thick portion of the oriented polymer composition adjacent to and below the de-oriented surface layer by sufficiently heat treating a surface of a cavitated oriented polymer composition.

REFERENCES:
patent: 5204045 (1993-04-01), Courval et al.
patent: 5474722 (1995-12-01), Woodhams
patent: 2004/0068848 (2004-04-01), Ausen et al.
patent: 2008/0111277 (2008-05-01), Nichols et al.
patent: 2008/0111278 (2008-05-01), Nichols et al.
patent: 2009/0001625 (2009-01-01), Newson et al.
patent: 2009/0001629 (2009-01-01), Newson et al.
patent: 2009/0001635 (2009-01-01), Newson et al.
patent: 1356916 (2003-10-01), None
patent: 1311885 (1973-03-01), None
patent: 2008057167 (2008-05-01), None
patent: WO2008/118643 (2008-10-01), None
U.S. Appl. No. 12/327,122, Bruce A. Malone, et al., filed Dec. 3, 2008, not published yet.
PCT/US2008/085210 WO/ISA Search Report and Written Opinion, Jan. 2010.
PCT/US2008/085210 Claims, Jan. 2010.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Oriented polymer composition with a deoriented surface layer does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Oriented polymer composition with a deoriented surface layer, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Oriented polymer composition with a deoriented surface layer will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4211711

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.