ABSTRACT:
Cobalt-base superalloys having special utility in the production of industrial gas turbine hot gas path components because of their unique combination of properties in specially heat-treated condition including excellent hot corrosion resistance, stress-rupture strength at high temperature, metallurgical stability, tensile ductility and weldability, consist essentially of 0.3 to 0.6% carbon, 27-35% chromium, 9-16% nickel, 6-9% tungsten, 0.45 to 2.0% tantalum, up to 3.0% hafnium, up to 0.7% zirconium, not more than 2.0% iron, 1.5% manganese and silicon and 0.05% boron, balance cobalt, the carbide formers being selected to satisfy the following equations: ##EQU1##
REFERENCES:
patent: 3118763 (1964-01-01), Thielemann
patent: 3314784 (1967-04-01), McQuillan et al.
patent: 3333957 (1967-08-01), Thielemann
patent: 3366478 (1968-01-01), Wheaton
patent: 3383205 (1968-05-01), Sims et al.
patent: 3432294 (1969-03-01), Wheaton
patent: 3549356 (1970-12-01), Sims et al.
patent: 3582320 (1971-06-01), Herchenroeder
patent: 3933484 (1976-07-01), Costin
patent: 4437913 (1984-03-01), Fukui et al.
Beltran Adrian M.
Haydon John S.
Wood John H.
Dear R.
General Electric Company
Squillaro Jerome C.
LandOfFree
Novel cobalt-base superalloy and cast and welded industrial gas does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Novel cobalt-base superalloy and cast and welded industrial gas , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Novel cobalt-base superalloy and cast and welded industrial gas will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1888523