In a non-oriented electromagnetic steel sheet including about 0.01 wt % or less of C, about 1.0 wt % or less of Si, Mn in a range of about 0.1 wt % to 1.5 wt %, Al in a range of about 0.2 wt % to 1.5 wt %; the steel sheet having a critical amount of about 2 to 80 ppm rare earth metal, and the quantities of Ti and Zr in the steel sheet being limited to about 15 ppm or less of Ti, and about 80 ppm or less of Zr. The sheet exhibits excellent magnetic characteristics, such as iron loss, even when punched and laminated sheets are stress relief annealed at a low temperature for a short period of time.

REFERENCES:
patent: 3960616 (1976-06-01), Evans et al.
patent: 4204890 (1980-05-01), Irie et al.
patent: 4338143 (1982-07-01), Shimoyama et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Non-oriented electromagnetic steel sheet with low iron loss afte does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Non-oriented electromagnetic steel sheet with low iron loss afte, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Non-oriented electromagnetic steel sheet with low iron loss afte will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-463169

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.