ABSTRACT:
Ink formulations have been conceived that result in inks having improved shelf life, tack and flow properties so that problems relating to ink plugging with contemporary ink pads are reduced. Another advantage of the inks is that they have improved paper dust resistance. These inks are made of a coloring material having an organic pigment dispersed in a modified rosin ester or dispersed in a modified rosin ester and triazine formaldehyde aryl sulphonamide resin dispersed in an alkyd oil. The solvent system is preferably composed of non drying solvents such as emollients and high molecular weight glycols.
REFERENCES:
patent: 2970965 (1961-02-01), Switzer
patent: 3928226 (1975-12-01), McDonough et al.
patent: 4361843 (1982-11-01), Cooke et al.
patent: 4386961 (1983-06-01), Lin
patent: 4400215 (1983-08-01), Cooke et al.
patent: 4531976 (1985-07-01), Lin
patent: 4767459 (1988-08-01), Greenwood et al.
patent: 4793264 (1988-12-01), Lin et al.
patent: 4822418 (1989-04-01), Lin et al.
patent: 5114478 (1992-05-01), Auslander et al.
Auslander Judith D.
Hochwalt Norman C.
Klemanski Helene
Pitney Bowes Inc.
Scolnick Melvin J.
Vrahotes Peter
LandOfFree
Non aqueous dispersion ink with improved shelf life, tack and fl does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Non aqueous dispersion ink with improved shelf life, tack and fl, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Non aqueous dispersion ink with improved shelf life, tack and fl will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-168294