ABSTRACT:
A solution polymerization system for polymerizing a olefin monomer by reacting the monomer with catalyst and solvent has been invented. The system in one aspect including a flow loop with a product polymer outlet, the flow loop forming a recycling reactor, a catalyst inlet on the flow loop through which catalyst and solvent flow into the flow loop, a monomer inlet on the flow loop through which monomer and solvent flow into the flow loop and, with the catalyst, form a reactant materials stream, a first heat exchanger on the flow loop for receiving the reactant materials stream and any formed polymer and for removing heat of reaction or polymerization from the flow loop, and pump apparatus for pumping the reactant materials stream and formed polymer in the flow loop and from the first heat exchanger to the product polymer outlet. In one aspect, the system includes at least one additional heat exchanger on the flow loop for receiving the reactant materials stream and formed polymer and for removing heat of reaction or polymerization from the flow loop, the pump apparatus pumping formed polymer and remaining reactant materials to the product polymer outlet, and a portion of the formed polymer and remaining reactant materials flowing out from the product polymer outlet and the remainder recycling through the flow loop. In one aspect systems and methods according to the present invention are used to make polyethylene.
REFERENCES:
patent: 3242150 (1966-03-01), Scoggin
patent: 4471095 (1984-09-01), Wassen et al.
patent: 5286884 (1994-02-01), Cowley et al.
Abstract No. 94-193111/24 (EP 0 602 509 A2), 1994.
Abstract No. 92-425517/52 (EP 0 519 266 A1), 1992.
Dissertation Abstract AAD89-15540, 1989.
Dissertation Abstract AAD84-10765, 1984.
Dissertation Abstract AAD83-04964, 1982.
Dissertation Abstract AAD82-26984, 1982.
D. A. Heierle, "Static mixer-heat exchangers", Chemical Plant & Processing, 1989.
C. E. Meyer, "Laminar Flow Static Mixing-Design and Scaleup Criteria", 1991 AlChe Annual Meeting, Los Angeles, Nov. 17-22, 1991 Session No. 119.
"Modernization of the TR. I De Solucion", Dow Chemical Iberica, S.A., Feb. 1995.
M. B. Welch et al., "Polyethylene Produced in Phillips Slurry Loop Reactors with Metallocene Catalysts", Worldwide Metallocene Conference MetCon '95 May 17-19, 1995.
Camp Gary A.
Combs R. Bruce
Eversdyk David A.
Jain Pradeep
Kao Che I.
The Dow Chemical Company
Wu David W.
LandOfFree
Non-adiabatic olefin solution polymerization does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Non-adiabatic olefin solution polymerization, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Non-adiabatic olefin solution polymerization will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2136528