ABSTRACT:
Methods for increasing the forgeability of cast superalloy materials are described. An extremely overaged microstructure is developed by solutionizing the material and slow cooling in the vicinity of the solvus temperature to cause a precipitation of extremely coarse gamma prime material. Subsequently the material can be isothermally forged.

REFERENCES:
patent: 3620855 (1971-11-01), Wagner et al.
patent: 3649379 (1972-03-01), Kotval
patent: 3676225 (1972-07-01), Owczarski et al.
patent: 3677830 (1972-07-01), Cox et al.
patent: 4392894 (1983-07-01), Pearson et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nickle base superalloy articles and method for making does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickle base superalloy articles and method for making, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickle base superalloy articles and method for making will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1593819

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.