ABSTRACT:
A nickel-chromium alloy excellent in a stress corrosion cracking resistance which is obtained by carrying out an annealing treatment under specific conditions, said alloy having the following composition:
REFERENCES:
patent: 3573901 (1971-04-01), Economy
Minami Takao
Nagano Hiroo
Okada Yasutaka
Onimura Kichiro
Sasaguri Nobuya
Dean R.
Mitsubishi Jukogyo Kabushiki Kaisha
Sumitomo Metal Industries Ltd.
LandOfFree
Nickel-chromium alloy in stress corrosion cracking resistance does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel-chromium alloy in stress corrosion cracking resistance, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-chromium alloy in stress corrosion cracking resistance will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-461503