Nickel/chrome base superalloys

Alloys or metallic compositions – Containing over 50 per cent metal but no base metal – Iron containing

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

Other Related Categories

65 15, 6537412, 420586, C22C 3000

Type

Patent

Status

active

Patent number

047088486

Description

ABSTRACT:
A nickel/chrome-base alloy, particularly suitable for high temperature molten glass handling and forming apparatus, resistant to oxidation and possessing high rupture strength.

REFERENCES:
patent: 4203748 (1980-05-01), Battigelli et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nickel/chrome base superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel/chrome base superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel/chrome base superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2423388

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.