ABSTRACT:
A nickel-based superalloy suitable for directed solidification, in particular for industrial gas turbine parts, having the following composition by weight:
REFERENCES:
patent: 3617261 (1971-02-01), Lherbier et al.
patent: 3969111 (1976-07-01), Acuncius et al.
patent: 4116723 (1978-09-01), Gell et al.
patent: 4379120 (1983-04-01), Whitney et al.
patent: 4388124 (1983-06-01), Henry
patent: 4492672 (1985-01-01), Duhl et al.
patent: 4830934 (1989-05-01), Ferrigno et al.
Caron Pierre
Khan Tasadduq
Naveos Serge
Raffestin Jean-Louis
Office National D'Etudes et de Recherches/Aerospatiales
Yee Deborah
LandOfFree
Nickel-based superalloy for industrial turbine blades does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel-based superalloy for industrial turbine blades, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-based superalloy for industrial turbine blades will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2379209