ABSTRACT:
A low density superalloy having good resistance to oxidation has the following composition by weight:

REFERENCES:
patent: 4837384 (1989-06-01), Khan et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nickel-based monocrystalline superalloy, in particular for the b does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel-based monocrystalline superalloy, in particular for the b, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-based monocrystalline superalloy, in particular for the b will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1166459

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.