ABSTRACT:
A low density superalloy having good resistance to oxidation has the following composition by weight:
Caron Pierre
Khan Tasadduq
Raffestin Jean-Louis
Dean R.
Dubno Herbert
Myers Jonathan
Office National d'Etudes et de Recherche Aerospatiales
LandOfFree
Nickel-based monocrystalline superalloy, in particular for the b does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel-based monocrystalline superalloy, in particular for the b, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-based monocrystalline superalloy, in particular for the b will most certainly appreciate the feedback.