ABSTRACT:
Nickel and iron-nickel base alloys are described together with a rapid solidification process used in the preparation thereof to provide materials useful in the fabrication of parts subject to high temperature operating conditions. The alloys include commercial nickel base superalloys to which a specified amount of boron is added.

REFERENCES:
patent: 3856513 (1974-12-01), Chen et al.
patent: 3871836 (1975-03-01), Polk et al.
patent: 4207098 (1980-06-01), Shaw

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nickel base superalloys which contain boron and have been proces does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel base superalloys which contain boron and have been proces, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel base superalloys which contain boron and have been proces will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1434789

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.