ABSTRACT:
There is provided by the present invention an alloy which is mechanically and chemically compatible with advanced nickel-base superalloys and nickel-base eutectic superalloys and which possesses excellent resistance to high temperature oxidation. The alloy of the invention is, therefore, particularly useful as a protective environmental coating for the external surfaces of hot-stage aircraft gas turbine engine components, e.g., rotating blades and stationary vanes, made from such advanced superalloys.
REFERENCES:
patent: 3276865 (1966-10-01), Fredie et al.
patent: 3526499 (1970-09-01), Quigg et al.
patent: 3904402 (1975-09-01), Smashey
patent: 3928026 (1975-12-01), Hecht et al.
patent: 4054723 (1977-10-01), Higginbottam et al.
patent: 4116723 (1978-09-01), Gell et al.
patent: 4169742 (1979-10-01), Wukusick et al.
patent: 4209348 (1980-06-01), Duhl et al.
patent: 4222794 (1980-09-01), Schweizer
patent: 4284430 (1981-08-01), Henry
patent: 4288247 (1981-09-01), Shaw
patent: 4292076 (1981-09-01), Gigliotti et al.
patent: 4313760 (1982-02-01), Dardi et al.
patent: 4326011 (1982-04-01), Goebel et al.
Gigliotti, Jr. Michael F. X.
Jackson Melvin R.
Prugar Mark L.
Rairden, III John R.
Yang Swe-Wong
General Electric Company
Lechert Jr. Stephen J.
Maria Carmen Santa
Squillaro Jerome C.
Strunck Stephen S.
LandOfFree
Nickel-base superalloys especially useful as compatible protecti does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel-base superalloys especially useful as compatible protecti, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-base superalloys especially useful as compatible protecti will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1542070