ABSTRACT:
The present invention provides an alloy having improved crack growth inhibition and having high strength at high temperatures. The composition of the alloy is essentially as follows:
REFERENCES:
patent: 3155501 (1964-11-01), Kaufman et al.
patent: 4039330 (1977-08-01), Shaw
patent: 4207098 (1980-06-01), Shaw
patent: 4519979 (1985-05-01), Shaw
patent: 4569824 (1986-02-01), Duhl et al.
patent: 4719080 (1988-01-01), Duhl et al.
patent: 4727740 (1988-03-01), Yabuki et al.
patent: 4777017 (1988-10-01), Khan et al.
patent: 4788036 (1988-11-01), Eiselstein et al.
Davis Jr. James C.
General Electric Company
Lechert Jr. Stephen J.
Magee Jr. James
Rochford Paul E.
LandOfFree
Nickel base superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel base superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel base superalloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1333025