ABSTRACT:
A nickel-base superalloy containing 14 to 22% chromium, 5 to 25% cobalt, 1 to 5% tungsten, 0.5 to 3% tantalum, 2 to 5% titanium, 1 to 4.5% aluminum, the sum of the titanium plus aluminum being 4.5 to 9%, up to 2% niobium, about 0.35 to 1.2% boron, up to 3.5% molybdenum, up to 0.5% zirconium, up to 0.2% total of yttrium and lanthanum, up to 0.1% carbon, at least 0.05% of at least one element of the group of hafnium and vanadium with the maximum being about 2.2% hafnium and 2% vanadium, the balance of the alloy being essentially nickel.

REFERENCES:
patent: 4127410 (1978-11-01), Merrick et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nickel-base superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel-base superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-base superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1190750

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.