ABSTRACT:
Nickel-base superalloy composition for the repair, coating or rebuilding of the surface of a superalloy substrate, such as a single crystal nickel-base superalloy, to impart thereto surface areas having improved high temperature properties such as hot corrosion resistance. The present compositions are applied by low heat-input welding processes, such as laser welding or plasma arc welding, and are formulated to provide hot corrosion resistance properties and yet to have good weldability properties. The composition contains, by weight percentages, 2-12.5 Cr, 6-17 Cr, 0.5-7 Mo, 0.5-4 Ta, 2.5-9.5 Al, 1-4 Re, 1.5-8.5 W, 0.01-2.5 Nb, 0.5-6 Ti, 0.01-0.7 Yt, 0.02-3.5 Hf, and balance Ni.

REFERENCES:
patent: 4388124 (1983-06-01), Henry
patent: 5068084 (1991-11-01), Cetel et al.
patent: 5077141 (1991-12-01), Naik et al.
patent: 5154884 (1992-01-01), Wukusick et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nickel-base superalloy compositions does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel-base superalloy compositions, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-base superalloy compositions will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1404473

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.