Specialized metallurgical processes – compositions for use therei – Compositions – Consolidated metal powder compositions
Patent
1977-04-04
1979-02-20
Hunt, Brooks H.
Specialized metallurgical processes, compositions for use therei
Compositions
Consolidated metal powder compositions
75 05C, 75211, 148 115P, 148 115H, B22F 300, B22F 100
Patent
active
041405285
ABSTRACT:
A nickel-base superalloy compacted fully dense article, produced by a powder metallurgy technique from prealloyed powder, said article being characterized by the absence of thermal induced porosity when heated at temperatures of at least 2200.degree. F and exhibiting improved superplastic behavior during forming operations, such as forging.
REFERENCES:
patent: 3681061 (1972-08-01), Flecher
patent: 3726722 (1973-04-01), Foerster
Hebeisen John C.
Thompson Vernon R.
Crucible Inc.
Hunt Brooks H.
LandOfFree
Nickel-base superalloy compacted articles does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel-base superalloy compacted articles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-base superalloy compacted articles will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-256743