ABSTRACT:
The present invention relates to a heat treated, gamma prime precipitation strengthened nickel base alloy having an improved resistance to hydrogen embrittlement, particularly crack propagation. The alloy has a microstructure which is essentially free of script carbides, gamma--gamma prime eutectic islands and porosity. The microstructure further includes a plurality of regularly occurring large barrier gamma prime precipitates and a continuous field of fine cuboidal gamma prime precipitates surrounding the large barrier gamma prime precipitates.
REFERENCES:
patent: 3403059 (1968-09-01), Barker et al.
patent: 3415641 (1968-12-01), Ross
patent: 3536542 (1970-10-01), Murphy et al.
patent: 3576681 (1971-04-01), Barker et al.
patent: 3642543 (1972-02-01), Owczarski et al.
patent: 3667938 (1972-06-01), Boesch
patent: 3677746 (1972-07-01), Lund et al.
patent: 3741824 (1973-06-01), Duvall et al.
patent: 3748192 (1973-07-01), Boesch
patent: 3915761 (1975-10-01), Tschinkel et al.
patent: 3973952 (1976-08-01), Bieber et al.
patent: 4083734 (1978-04-01), Boesch
patent: 4253884 (1981-03-01), Maurer et al.
patent: 4305761 (1981-12-01), Bruch et al.
patent: 4379120 (1983-04-01), Whitney et al.
patent: 4461659 (1984-07-01), Harris
patent: 4512817 (1985-04-01), Duhl et al.
patent: 4518442 (1985-05-01), Chin
patent: 4676846 (1987-06-01), Harf
patent: 4717432 (1988-01-01), Ault
patent: 4795507 (1989-01-01), Nazmy
patent: 4878952 (1989-11-01), Pilloefer
patent: 4957567 (1990-09-01), Krueger et al.
patent: 5047091 (1991-09-01), Khan et al.
patent: 5061324 (1991-10-01), Keh-Minn Chang
patent: 5100484 (1992-03-01), Wukusick et al.
patent: 5143563 (1992-09-01), Krueger et al.
patent: 5328659 (1994-07-01), Tillman et al.
patent: 5413752 (1995-05-01), Kissinger et al.
D. P. DeLuca, R. W. Hatala "Single Crystal PWA 1472 in High Pressure Hydrogen" 10 pgs.
The Effect of Internal Hydrogen on a Single-Crystal Nickel-Base Superalloy, W.S. Walston, I.M. Bernstein and A.W. Thompson, Metallurgical Transastions A, vol. 23A, Apr. 1992, pp. 1313-1322.
Journal of Materals Science; 29 (1994) 2445-2458.
Metallurgical Trans A 3 2157-2162, Aug. 1972.
Metal Alloys Index 92(2):31-885, Feb. 1972.
Metal Alloys Index 94 (3): 31-1378, Mar. 1994.
DeLuca et al; Superalloys 718, 625. 706 Var Deriv., Proc. Int. Symp., 3rd (1994), 817-26.
Biondo Charles M.
DeLuca Daniel P.
Jones Howard B.
Rhemer Chris C.
Phipps Margery S.
Simmons David A.
United Technologies Corporation
LandOfFree
Nickel base superalloy articles with improved resistance to crac does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel base superalloy articles with improved resistance to crac, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel base superalloy articles with improved resistance to crac will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-135955