Nickel base superalloy articles and method for making

Metal treatment – Compositions – Heat treating

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148 115N, 148 127N, 148410, 148428, C22F 110

Patent

active

047690879

ABSTRACT:
A process is described for converting a fine grain superalloy casting into a forging having mechanical properties equivalent to those resulting from powder metallurgy processing. Cast material is extruded and forged. A HIP treatment is employed to close porosity.

REFERENCES:
patent: 3529503 (1970-09-01), Sederberg et al.
patent: 3620855 (1971-11-01), Wagner et al.
patent: 3649379 (1972-03-01), Kotval
patent: 3676225 (1972-07-01), Owczarski et al.
patent: 3677830 (1972-07-01), Cox et al.
patent: 3802938 (1974-04-01), Collins et al.
patent: 3975219 (1976-08-01), Allen et al.
patent: 4081295 (1978-03-01), Vogel
patent: 4110131 (1978-08-01), Gessinger
patent: 4392894 (1983-07-01), Pearson et al.
patent: 4574015 (1986-03-01), Genereux et al.
patent: 4579602 (1986-04-01), Paulonis et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nickel base superalloy articles and method for making does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel base superalloy articles and method for making, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel base superalloy articles and method for making will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1605038

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.