ABSTRACT:
A nickel base superalloy capable of being made into a single crystal article is provided with high temperature strength and improved stability by limiting the Presence of an undesirable SRZ constituent. Significant to the control of formation of such undesirable constituents is the control of the amount of Re in the alloy in combination with elements such as Al, Cr, Ta, Mo, Co and W. A solution heat treatment is provided for additional control.

REFERENCES:
patent: 3904402 (1975-09-01), Smashey
patent: 4031945 (1977-06-01), Gigliotti et al.
patent: 4116723 (1978-09-01), Gell et al.
patent: 4162918 (1979-07-01), Huseby
patent: 4169742 (1979-10-01), Wukusick et al.
patent: 4522664 (1985-06-01), Gigliotti et al.
patent: 4589937 (1986-05-01), Jackson et al.
patent: 4719080 (1988-01-01), Duhl et al.
patent: 4849030 (1989-07-01), Darolia et al.
patent: 5077141 (1991-12-01), Naik et al.
patent: 5100484 (1992-03-01), Wukusick et al.
patent: 5151249 (1992-09-01), Austin et al.
patent: 5154884 (1992-10-01), Wukusick et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nickel-base superalloy and article with high temperature strengt does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel-base superalloy and article with high temperature strengt, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-base superalloy and article with high temperature strengt will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1703968

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.