ABSTRACT:
In section bars and shaped bodies made of nickel-base superalloys having a structure consisting of columnar grains, a complete recrystallization cannot be effected unless the heating-up rate is kept below a maximum heating-up rate T.sub.max, which depends on the ratio V of one or more of the metal carbide-forming elements hafnium, niobium, tantalum, titanium and zirconium to one or both of the metal carbide-forming elements tungsten and molybdenum.
REFERENCES:
patent: 3368888 (1968-02-01), Winter et al.
patent: 3890816 (1975-06-01), Allen et al.
patent: 5154884 (1992-10-01), Wukusick et al.
Rosenberg, Samuel, "Nickel and Its Alloys", U.S. Dept of Commerce, 1968, pp. 74-78.
Fischmeister Hellmut
Lempenauer Klaus
Zoltzer Klaus
Jenkins Daniel
PM Hochtemperatur-Metall GmbH
Walsh Donald P.
LandOfFree
Nickel-base superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel-base superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-base superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1533063