ABSTRACT:
A nickel-base single crystal superalloy having high creep rupture strength at high temperatures, said superalloy being obtained by subjecting a single crystal alloy having a composition consisting essentially of, by weight,
REFERENCES:
patent: 4116723 (1978-09-01), Gell et al.
Harada Hiroshi
Yamagata Toshihiro
Yamazaki Michio
Dean R.
National Research Institute for Metals
LandOfFree
Nickel-base single crystal superalloy and process for production does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel-base single crystal superalloy and process for production, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-base single crystal superalloy and process for production will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1447758