ABSTRACT:
The invention is an indenter tip that is modified to permit both compression testing and tensile testing on samples having dimensions smaller than approximately 1 μm. The modified indenter tip has both a surface that can be used to apply compressive forces, and tines that can be used to engage a free end of a specimen to be tested in tension. The apparatus used to perform the tests includes elements of a scanning electron microscope that permit visualization of the specimen to be tested and the modified indenter tip, so as to permit appropriate alignment and engagement of the same. The apparatus also includes elements of a microindenter that provide mechanical manipulation of the relative position and orientation of the modified indenter tip and of the specimen to be tested, as well as the necessary controls and instrumentation to perform the test and to collect, record and manipulate data.

REFERENCES:
patent: 7444880 (2008-11-01), Zhang et al.
patent: 7681459 (2010-03-01), Yang et al.
patent: 7752916 (2010-07-01), Han et al.
patent: 2004/0144180 (2004-07-01), Imamura
patent: 2009/0164161 (2009-06-01), Hong et al.
patent: 2010/0122572 (2010-05-01), Scherzinger et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Nanoindenter tip for uniaxial tension and compression testing does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nanoindenter tip for uniaxial tension and compression testing, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nanoindenter tip for uniaxial tension and compression testing will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2646140

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.