Multiple domain fibers having surface roughened or mechanically

Stock material or miscellaneous articles – Coated or structually defined flake – particle – cell – strand,... – Rod – strand – filament or fiber

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

428374, 428397, D02G 300

Patent

active

059224622

ABSTRACT:
Multicomponent fiber and a method of producing the same whereby the inter-domain boundary layer between the distinct domains is surface roughened and/or mechanically modified so as to increase the surface area contact (and thereby the adhesion) therebetween. As such, delamination of the domains at their interfacial boundary layer is minimized (if not eliminated entirely). Preferably, the fibers are concentric core-sheath bicomponent fibers whereby the core is surface roughened and/or mechanically modified so that of the inter-domain boundary layer between the core and the sheath appears in cross-section to be serrated, undulated and/or ribbed so as to provide a core domain with a shape factor of between about 25 to about 55.

REFERENCES:
patent: 2989798 (1961-06-01), Bannerman
patent: 3718534 (1973-02-01), Okamoto et al.
patent: 4069363 (1978-01-01), Segraves et al.
patent: 4439487 (1984-03-01), Jennings
patent: 4460649 (1984-07-01), Park et al.
patent: 4732809 (1988-03-01), Harris et al.
patent: 4956236 (1990-09-01), Wang
patent: 5125818 (1992-06-01), Yeh et al.
patent: 5162074 (1992-11-01), Hills
patent: 5202185 (1993-04-01), Samuelson
patent: 5244614 (1993-09-01), Hagen
patent: 5344297 (1994-09-01), Hills
patent: 5352518 (1994-10-01), Muramoto et al.
patent: 5445884 (1995-08-01), Hoyt et al.
patent: 5533883 (1996-07-01), Hodan et al.
patent: 5551588 (1996-09-01), Hills
patent: 5582913 (1996-12-01), Simons
patent: 5780156 (1998-07-01), Hoyt et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Multiple domain fibers having surface roughened or mechanically does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Multiple domain fibers having surface roughened or mechanically , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Multiple domain fibers having surface roughened or mechanically will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2274389

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.