ABSTRACT:
In a multilayer ceramic circuit board comprising a substrate, an insulating layer on the substrate, and a conductive pattern on the insulating layer, an additive of Cr.sub.2 O.sub.3 or MnO.sub.2 is added to the insulating layer to reinforce adhesion between the insulating layer and the conductive pattern. Each of the substrate and the insulating layer is manufactured by firing at a temperature between 800.degree. C. and 1000.degree. C., alumina particles and a glass composition comprising an alumina component. When a total amount of alumina in the substrate is equal to or greater than that in the insulating layer, an amount of Cr.sub.2 O.sub.3 or MnO.sub.2 is restricted to a range between 0.1% and 10.0% by weight, with a difference between the total amounts of alumina falling within a range between 0% and 30% by weight. When the total amount of alumina in the substrate is smaller than that in the insulating layer, the amounts of Cr.sub.2 O.sub.3 and MnO.sub.2 may be between 0.1% and 10.0% by weight and between 0.1% and 15% by weight, respectively. The difference between the total amounts of alumina may be between 0% and 20% by weight.

REFERENCES:
patent: 4401766 (1983-08-01), Kyle

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Multilayer ceramic circuit board fired at a low temperature does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Multilayer ceramic circuit board fired at a low temperature, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Multilayer ceramic circuit board fired at a low temperature will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1873901

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.