ABSTRACT:
Coercivity of ferromagnetic particles is increased by depositing multiple layrs containing transition metals, including cobalt, on the surface of the particles at ambient temperature. Thereafter, the particles are heated sufficiently to obtain the desired level of coercivity. Typically, total heating time is five to ten hours.
Pianalto Bernard D.
Tandy Corporation
LandOfFree
Multi-layer process for cobalt treatment of ferromagnetic oxides does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Multi-layer process for cobalt treatment of ferromagnetic oxides, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Multi-layer process for cobalt treatment of ferromagnetic oxides will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1801791