Multi-laser beam welding high strength superalloys

Electric heating – Metal heating – By arc

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C148S525000, C219S121630

Reexamination Certificate

active

06972390

ABSTRACT:
A method is provided for repairing degraded and/or eroded areas on gas turbine blades and vanes. The method is directed to turbine blades and vanes made of advanced superalloy materials with high elevated-temperature properties. The method uses multiple laser beams to perform steps of preheating the repair area, welding the repair area, and post-welding heating of the repaired area. The method uses an array of two or more lasers to perform the steps of heating, welding, and post-weld heat treatment in nearly simultaneous operation thereby dramatically reducing or eliminating the hot cracking associated with other welding methods used with superalloy materials. The method is further directed to cladding or material buildup of degraded turbine blades where the weld material is the same as the matrix or better superalloy materials.

REFERENCES:
patent: 4804815 (1989-02-01), Everett
patent: 5106010 (1992-04-01), Stueber et al.
patent: 5308409 (1994-05-01), Kamimura et al.
patent: 5554837 (1996-09-01), Goodwater et al.
patent: 5914059 (1999-06-01), Marcin et al.
patent: 6054672 (2000-04-01), Foster et al.
patent: 6191379 (2001-02-01), Offer et al.
patent: 6269540 (2001-08-01), Islam et al.
patent: 6364971 (2002-04-01), Peterson, Jr. et al.
patent: 6596411 (2003-07-01), Feng et al.
patent: 2005/0028897 (2005-02-01), Kurz et al.
patent: 2001-269784 (2001-10-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Multi-laser beam welding high strength superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Multi-laser beam welding high strength superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Multi-laser beam welding high strength superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3476421

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.