Thermal measuring and testing – Heat flux measurement – By differential temperature measurement along undisturbed...
Reexamination Certificate
2007-09-11
2009-08-25
Verbitsky, Gail (Department: 2855)
Thermal measuring and testing
Heat flux measurement
By differential temperature measurement along undisturbed...
C374S011000, C374S141000, C422S051000, C436S147000
Reexamination Certificate
active
07578613
ABSTRACT:
A modulated differential scanning calorimeter that accounts for heat flow due to evaporative solvent loss. The calorimeter modulates the temperature applied to a sample and a reference to determine the amount of heat flow that is due to evaporation. By calculating the amount of heat flow due to evaporation, the user can determine how much of the heat flow of any given well is due to the process of interest as opposed to evaporation.
REFERENCES:
patent: 3467501 (1969-09-01), Groszek
patent: 4812051 (1989-03-01), Paulik et al.
patent: 5224775 (1993-07-01), Reading et al.
patent: 5255976 (1993-10-01), Connelly
patent: 5335993 (1994-08-01), Marcus et al.
patent: 5451371 (1995-09-01), Zanini-Fisher et al.
patent: 5967659 (1999-10-01), Plotnikov et al.
patent: 6193413 (2001-02-01), Lieberman
patent: 6535824 (2003-03-01), Mansky et al.
patent: 6561692 (2003-05-01), Danley
patent: 6602714 (2003-08-01), Tagge et al.
patent: 6869214 (2005-03-01), Plotnikov et al.
patent: 7033840 (2006-04-01), Tagge et al.
patent: 2005/0036536 (2005-02-01), Lewis
patent: 2005/0107959 (2005-05-01), Zhang
patent: 2005/0141587 (2005-06-01), Muhlig et al.
International Search Report dated May 12, 2008.
Baghdadi Aslan
Paul, Hasting, Janofsky & Walker LLP
Verbitsky Gail
Waters Investments Limited
LandOfFree
Modulated differential scanning calorimeter solvent loss... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Modulated differential scanning calorimeter solvent loss..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Modulated differential scanning calorimeter solvent loss... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4062977