Mixing procedure for obtaining filled rubber vulcanizates contai

Resilient tires and wheels – Tires – resilient – Pneumatic tire or inner tube

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

152374R, 524 87, 524 89, 524 91, 524 92, 524 94, 524496, 525194, 525233, 525347, 525375, 525377, 525381, C08C 400, C08K 535, C08K 304

Patent

active

045706905

ABSTRACT:
Filled rubber vulcanizates containing aromatic furazan oxides exhibit many improved properties such as increased filler-rubber interaction and decreased hysteresis. Useful furazan oxides have both carbons of the furazan ring as part of a fused aromatic ring. Typical examples are benzofurazan oxide and its methyl and methoxy analogs. Tires made from the inventive vulcanizates show lower running temperatures and improved rolling resistance. The desirable effects of the aromatic furazan oxides may be improved by mixing the rubber, filler and furazan oxide in a conventional mechanical compounding device at specific temperatures and time periods such as about 200.degree.-400.degree. F. for 2-20 minutes.

REFERENCES:
patent: 3931106 (1976-01-01), Crosby

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Mixing procedure for obtaining filled rubber vulcanizates contai does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Mixing procedure for obtaining filled rubber vulcanizates contai, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Mixing procedure for obtaining filled rubber vulcanizates contai will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1545896

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.