ABSTRACT:
Mixed oxide compounds La.sub.2 O.sub.3 . 11Al.sub.2 O.sub.3, NdAlO.sub.3 and nonstoichiometric MgAl.sub.2 O.sub.3 are suitable for making cores and molds for casting advanced superalloy materials such as NiTaC-13.
REFERENCES:
patent: 3420780 (1969-01-01), Forrat et al.
patent: 3725094 (1973-04-01), Levy, Jr. et al.
patent: 4031177 (1977-06-01), Auriol et al.
Huseby Irvin C.
Klug Frederic J.
Bell Mark
Cohen Joseph T.
General Electric Company
Vertiz O. R.
Watts Charles T.
LandOfFree
Mixed oxide compounds for casting advanced superalloy materials does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Mixed oxide compounds for casting advanced superalloy materials, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Mixed oxide compounds for casting advanced superalloy materials will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1555636