Mitigation of stress corrosion cracking of structural...

Chemical apparatus and process disinfecting – deodorizing – preser – Process disinfecting – preserving – deodorizing – or sterilizing – Maintaining environment nondestructive to metal

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C422S011000, C422S012000, C422S014000, C422S019000, C376S277000, C376S305000, C376S306000

Reexamination Certificate

active

11120478

ABSTRACT:
A method for mitigating stress corrosion cracking of a component exposed to a high temperature water in a high temperature water system is provided. The method comprises the steps of lowering corrosion potential conditions to a desired low corrosion potential in the high temperature water environment; and introducing a first material comprising zinc into the high temperature water environment, such that the desired low corrosion potential facilitates transport of the first material into cracks in a structure communicative with the high temperature water environment.

REFERENCES:
patent: 5673297 (1997-09-01), Andresen
patent: 6714618 (2004-03-01), Hettiarachchi et al.
patent: 6793883 (2004-09-01), Andresen et al.
patent: 2002/0101953 (2002-08-01), Hettiarachchi et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Mitigation of stress corrosion cracking of structural... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Mitigation of stress corrosion cracking of structural..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Mitigation of stress corrosion cracking of structural... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3727120

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.