ABSTRACT:
A method for producing a tubular bar, more particularly a stabilizer bar, is provided. The method comprises providing a tubular bar of desired size having an outer and inner surface, heating the bar to an elevated temperature, quenching the bar by application of a cooling fluid to the surfaces of the bar, and forming the tube to a desired shape without annealing. The method further provides for the composition of a high-strength, high formability carbon steel alloy to be used in conjunction with the method. Advantageously, the bar is formable without thermal processing subsequent to quenching. In this fashion, metal tubular bars, such as stabilizer bars, may be formed at reduced cost.

REFERENCES:
patent: 4231555 (1980-11-01), Saito
patent: 4336081 (1982-06-01), Hijikata et al.
patent: 4376528 (1983-03-01), Ohshimatani et al.
patent: 4526628 (1985-07-01), Ohno et al.
patent: 5538566 (1996-07-01), Gallagher
patent: 5598735 (1997-02-01), Saito et al.
patent: 6196530 (2001-03-01), Muhr et al.
patent: 6311965 (2001-11-01), Muhr et al.
patent: 6384388 (2002-05-01), Anderson et al.
patent: 6682610 (2004-01-01), Inoue
patent: 2004/0131876 (2004-07-01), Ohgami et al.
patent: 2004/0139780 (2004-07-01), Cai et al.
patent: 2005/0087269 (2005-04-01), Merwin
patent: 2006/0243355 (2006-11-01), Haiderer et al.
patent: 0 092 815 (1983-11-01), None
patent: 0 753 595 (1997-01-01), None
patent: 1 717 324 (2006-11-01), None
patent: 2001-164338 (2001-06-01), None
Mechanical Tubing and Cold Finishing, Metals Handbook Desk Edition, (2000), 5 pages.
English translation of JP 2001-164338 to Sato et al, published Jun. 2001, 31 pages.
Beretta, Stefano et al., “Fatigue Assessment of Tubular Automotive Components in Presence of Inhomogeneities”, Proceedings of IMECE2004, ASME International Mechanical Engineering Congress, Nov. 13-19, 2004, pp. 1-8.
Prevey, Paul, et al., “Introduction of Residual Stresses to Enhance Fatigue Performance in the Initial Design”, Proceedings of Turbo Expo 2004, Jun. 14-17, 2004, pp. 1-9.
International Search Report and Written Opinion for PCT/IB2007/001995 (corresponding PCT application to U.S. Appl. No. 11/375,660) dated Dec. 21, 2007.
Corrected International Preliminary Report on Patentability for PCT/IB2007/001995 (corresponding to PCT application to U.S. Appl. No. 11/375,660) dated Sep. 10, 2008.
International Preliminary Report on Patentability for PCT/IB2007/001995 (corresponding to PCT application to U.S. Appl. No. 11/375,660) dated Jul. 17, 2008.
Wegst, C.W., “Stahlschlüssel”, Auflage 1989, Seite 119, Published 1989.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Methods of producing high-strength metal tubular bars... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Methods of producing high-strength metal tubular bars..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Methods of producing high-strength metal tubular bars... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4153901

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.