ABSTRACT:
Refractory uranium is crushed and impregnated with a concentrated aqueous solution of sulphuric acid to provide a mixture which retains a solid phase consistency. The impregnated mixture is disintegrated in an aqueous solution to form a thick paste or pulp. The pulp is digested for a duration not exceeding 10 hours and the uranium recovered by solid/liquid separation. The sulphuric acid content of the concentrated solution is selected for the residual acidity at the end of pulp digestion to be of from 10 g/l to 40 g/l.

REFERENCES:
patent: 2830872 (1958-04-01), McCullough
patent: 2849280 (1958-08-01), Baron et al.
patent: 3808306 (1974-04-01), Smith et al.
patent: 4098866 (1978-07-01), Carnahan et al.
patent: 4131639 (1978-12-01), Mather
patent: 4175108 (1979-11-01), Poitte

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Methods of processing uraniferous ores does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Methods of processing uraniferous ores, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Methods of processing uraniferous ores will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1292201

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.