ABSTRACT:
This invention relates to a method to process narrow molecular weight distribution polyolefins, particularly thermoplastics, polyethylenes, polypropylenes, and polyacrylates, whether they are homopolymers or copolymers. The process may be used in any extruder and is typically implemented along the extruder screw and/or barrel by heating the first zone the screw/barrel to place the polyolefin into a molten, flowable state. Thereafter, the polymer is cooled in the second heating zone to a point 50.degree. C. above or 10.degree. C. below the crystalline melting temperature of the polymer and thereafter is reheated in the final heating zone to a molten, flowable state and finally extruding it within 5 seconds or less through the die.

REFERENCES:
patent: 4452977 (1984-06-01), Brasz et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method to process narrow molecular weight distribution polyolefi does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method to process narrow molecular weight distribution polyolefi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method to process narrow molecular weight distribution polyolefi will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1659644

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.