Wells – Processes – With indicating – testing – measuring or locating
Patent
1990-09-07
1992-05-12
Suchfield, George A.
Wells
Processes
With indicating, testing, measuring or locating
166281, 166297, 166308, E21B 43267, E21B 4900
Patent
active
051118815
ABSTRACT:
This invention relates to a procedure to control fracture orientation in underground formations to increase well productivity. The method is performed by hydraulically fracturing the formation and propping and plugging the fractures which result. The formation is then perforated or notched in a direction angularly disposed relative to the anticipated fracture formation and first hydraulic fracture. The presence of the first fracture will force the second fracture to propagate in a direction away from that of the first fracture. A method for simultaneously fracturing the formation in two directions is also provided.
REFERENCES:
patent: 3289762 (1966-12-01), Schell et al.
patent: 3537529 (1970-11-01), Timmerman
patent: 4005750 (1977-02-01), Shuck
patent: 4669546 (1987-06-01), Jennings, Jr. et al.
patent: 4687061 (1987-08-01), Uhri
patent: 4718490 (1988-01-01), Uhri
patent: 4724905 (1988-02-01), Uhri
patent: 4830106 (1989-05-01), Uhri
patent: 4834181 (1989-05-01), Uhri et al.
patent: 4850431 (1989-07-01), Austin et al.
patent: 4869322 (1989-09-01), Vogt, Jr. et al.
patent: 4974675 (1990-12-01), Austin et al.
patent: 4977961 (1990-12-01), Avasthi
Warpinski et al., Altered-Stress Fracturing, SPE 17533 (presented at SPE Rocky Mountain Regional Meeting, Casper, Wyo., May 11-13, 1988).
Kuhlman, Microfrac Tests Optimize Frac Jobs, Oil & Gas Journal, 45-49 (Jan. 1990).
Daneshy et al., In-Situ Stress Measurements During Drilling, Journal of Petroleum Technology, 891-898 (Aug. 1986).
L. W. Teufel, Determination of In-Situ Stress from Anelastic Strain Recovery Measurements of Oriented Core, SPE/DOE 11649, Mar. 1983.
Sneddon and Elliot, The Opening of a Griffith Crack Under Internal Pressure, Quarterly of Applied Mathematics, vol. 4, No. 3, p. 262 (1946).
Green and Sneddon, Distribution of Stress in the Neighborhood of a Flat Elliptical Crack of an Elastic Solid, Proceedings Cambridge Phil. Soc. pp. 159-163 (Jan. 1949).
Daneshy A. Ali
Soliman Mohamed Y.
Venditto James J.
Halliburton Company
Kent Robert A.
Suchfield George A.
LandOfFree
Method to control fracture orientation in underground formation does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method to control fracture orientation in underground formation, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method to control fracture orientation in underground formation will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2423608