Metal fusion bonding – Process – Using dynamic frictional energy
Reexamination Certificate
2011-05-31
2011-05-31
Stoner, Kiley (Department: 1735)
Metal fusion bonding
Process
Using dynamic frictional energy
C228S160000, C228S170000
Reexamination Certificate
active
07950566
ABSTRACT:
A method of processing heated metal logs in a metal extrusion process. The remainder of each log is attached to the succeeding log. Specifically, the abutted ends of the two log segments are aligned with a saw. The saw is actuated to simultaneously remove material from both of the abutted ends. The cut ends are friction welded together through relative rotation of the log segments. The process creates a heated log column that is effectively endless, eliminating log remainders.
REFERENCES:
patent: 2187740 (1940-01-01), Hothersall
patent: 2912563 (1959-11-01), Schlieker et al.
patent: 3062249 (1962-11-01), Gray
patent: 3198931 (1965-08-01), Klempay
patent: 3369385 (1968-02-01), Murphy et al.
patent: 3394213 (1968-07-01), Roberts et al.
patent: 3394857 (1968-07-01), Wheeler et al.
patent: 3769124 (1973-10-01), Johnson
patent: 3816696 (1974-06-01), Wheeler et al.
patent: 3984652 (1976-10-01), Graville
patent: 4651602 (1987-03-01), Harrold et al.
patent: 4679475 (1987-07-01), Antezana
patent: 4787281 (1988-11-01), Gardner
patent: 4840303 (1989-06-01), Fujii et al.
patent: 4901611 (1990-02-01), Bentley
patent: 5062299 (1991-11-01), Davis et al.
patent: 5532451 (1996-07-01), La Rocca
patent: 5709585 (1998-01-01), Matsuo et al.
patent: 5836190 (1998-11-01), Wompner et al.
patent: 6893531 (2005-05-01), Todaro et al.
patent: 2002/0011469 (2002-01-01), Miyata et al.
patent: 2004/0231391 (2004-11-01), Wompner et al.
patent: 2005/0034502 (2005-02-01), Kohn
patent: 3120464 (1982-09-01), None
patent: 10232608 (2003-01-01), None
patent: 202004008241 (2004-12-01), None
patent: 102006007850 (2007-08-01), None
patent: 0065933 (1982-12-01), None
patent: 0244063 (1987-11-01), None
patent: 0467875 (1992-01-01), None
patent: 0787543 (1997-01-01), None
patent: 0791409 (1997-08-01), None
patent: 1463020 (1977-02-01), None
patent: 5581017 (1980-06-01), None
patent: 57154313 (1982-09-01), None
patent: 58034715 (1983-03-01), None
patent: 03193207 (1991-03-01), None
patent: 06007968 (1994-01-01), None
patent: 2002224707 (2002-08-01), None
patent: 2002224856 (2002-08-01), None
patent: 2004-34254 (2004-02-01), None
patent: 0178935 (2001-10-01), None
Notification of Transmittal of the International Search Report and the Written Opinion of the International Searching Authority, or the Declaration, International Search Report, Written Opinion of the International Searching Authority, mailed Jan. 22, 2009.
Boden Derek William
Buiten Scott David
G. James Australia Pty. Ltd.
Granco Clark, Inc.
Stoner Kiley
Warner & Norcross & Judd LLP
LandOfFree
Method of welding heated log segments in an aluminum... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of welding heated log segments in an aluminum..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of welding heated log segments in an aluminum... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2702472