ABSTRACT:
Aluminum is joined to titanium by welding using so much welding energy that the temperature on the titanium side of the alloying melt boundary remains below 2000.degree. C., while titanium and aluminum do, however, melt at the joint interface.
In a weldment thus obtained, the base material alloys and aluminum filler of which contain at maximum 10% titanium, there is in the vicinity of the interface between titanium and aluminum only a discontinuous .beta.-phase, dispersed in the aluminum matrix.

REFERENCES:
patent: 2761047 (1956-08-01), Meredith
patent: 3473216 (1969-10-01), Webb
American Society for Metals, Metals Handbook, 8th Edition, vol. 6, Welding and Brazing, 1971, p. 375.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of welding aluminum to titanium and a welded joint so pro does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of welding aluminum to titanium and a welded joint so pro, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of welding aluminum to titanium and a welded joint so pro will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1584180

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.