ABSTRACT:
A structural member to be subjected to a hot gas atmosphere produced through reaction between coal and a gasifier such as oxygen, air, steam or hydrogen, in a gasification furnace for example. The structural member is made of an anti-sulfur attack Cr-Ni-Al-Si alloy steel which has a composition essentially consisting of, by weight, 0.03 to 0.3% of C, 1 to 10% of Si, not greater than 2.0% of Mn, 8 to 14% of Ni, 16 to 20% of Cr, 0.5 to 10% of Al and the balance not less than 50% of Fe.

REFERENCES:
patent: 1538360 (1919-02-01), Smith
patent: 4108641 (1978-08-01), Fujioka et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of using a structural member of anti-sulfur-attack cr-ni- does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of using a structural member of anti-sulfur-attack cr-ni-, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of using a structural member of anti-sulfur-attack cr-ni- will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1082695

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.