ABSTRACT:
In the surface treatment of copper and its alloys with an acidic aqueous solution of hydrogen peroxide, methylcyclohexanol or cyclohexanol or both of the two are added to the solution thereby inhibiting the hindering action of chlorine ion in removal of metals and oxide scales by dissolution.
REFERENCES:
patent: 3293093 (1966-12-01), Jones et al.
patent: 3483050 (1969-12-01), Banush
patent: 3556883 (1971-01-01), Naito et al.
patent: 3597290 (1971-08-01), Naito et al.
patent: 3635836 (1972-01-01), Mullen
patent: 3649194 (1972-03-01), Glanville
patent: 3864271 (1975-02-01), Stalter
patent: 3869401 (1975-03-01), Ernst
patent: 3905907 (1975-09-01), Shiga
Bashore S. Leon
Caroff Marc L.
Tokai Denka Kogyo Kabushiki Kaisha
LandOfFree
Method of treating surface of copper and its alloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of treating surface of copper and its alloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of treating surface of copper and its alloys will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1226033