ABSTRACT:
The method consists in preparing a mixture composed of 20-80 g of molybdenum disulphide and 1-5 g of sulphuric acid per liter of glycerine, heating said mixture from 180.degree. to 230.degree. C, holding the workpieces in said mixture for 3-7 hours in presence of brass, followed by washing the parts with a cooling liquid and drying them.

REFERENCES:
patent: 2609342 (1952-09-01), White et al.
patent: 2622993 (1952-12-01), McCullough
patent: 2905574 (1959-09-01), Spengler

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of surface-strengthening of steel parts working in abrasi does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of surface-strengthening of steel parts working in abrasi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of surface-strengthening of steel parts working in abrasi will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-103295

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.