Method of stress-relief annealing a magnetic core containing amo

Metal treatment – Process of modifying or maintaining internal physical... – Magnetic materials

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148108, 29605, 29609, 296021, 219 1041, 219 1057, H01F 100

Patent

active

048327638

ABSTRACT:
A method of stress-relief annealing a magnetic core constructed of magnetic, metallic strip material, with at least a portion of the strip material being amorphous, wherein the strip material has major plane surfaces which define first exposed surfaces of the magnetic core, and lateral edges which collectively define second exposed surfaces of the magnetic core. The method includes the step of thermally insulating the first exposed surfaces of the magnetic core, and the step of heating the magnetic core via the second exposed surfaces.

REFERENCES:
patent: 4262233 (1981-04-01), Becker et al.
patent: 4298409 (1981-11-01), DeCristofaro et al.
patent: 4512924 (1985-04-01), Taub
patent: 4529177 (1985-07-01), Sheth et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of stress-relief annealing a magnetic core containing amo does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of stress-relief annealing a magnetic core containing amo, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of stress-relief annealing a magnetic core containing amo will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1728514

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.