Method of stress corrosion cracking mitigation for nuclear...

Induced nuclear reactions: processes – systems – and elements – Reactor protection or damage prevention – Corrosion or damage prevention

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C376S306000

Reexamination Certificate

active

07864914

ABSTRACT:
The object of this invention is to provide a method for mitigating a stress corrosion cracking of reactor structural material which makes it possible to suppress the rise in the main steam line dose rate without secondary effects such as a rise in the concentration of radioactive cobalt-60, etc. in the reactor water. Hydrogen and a reductive nitrogen compound containing nitrogen having a negative oxidation number (for example, hydrazine) are injected into the core water of boiling water nuclear power plant. By injecting the reductive nitrogen compound containing nitrogen having a negative oxidation number into the core water, the stress corrosion cracking of structural material of reactor can be mitigated without side reactions such as a rise in the concentration of cobalt-60, etc.

REFERENCES:
patent: 3294644 (1966-12-01), Walton
patent: 4376753 (1983-03-01), Lucas
patent: 5084235 (1992-01-01), Ibe et al.
patent: 5135709 (1992-08-01), Andresen et al.
patent: 5164152 (1992-11-01), Kim et al.
patent: 5203984 (1993-04-01), Sakai et al.
patent: 5398268 (1995-03-01), Ibe et al.
patent: 5448605 (1995-09-01), Hettiarachchi
patent: 5600692 (1997-02-01), Hettiarachchi
patent: 6724854 (2004-04-01), Kim et al.
patent: 6793883 (2004-09-01), Andresen et al.
patent: 2002/0080906 (2002-06-01), Andresen et al.
patent: 2002/1118787 (2002-08-01), Andresen et al.
patent: 2003/0012686 (2003-01-01), Andresen et al.
patent: 7209487 (1995-08-01), None
patent: 08327786 (1996-12-01), None
patent: 2766422 (1998-04-01), None
patent: 2001525494 (2001-12-01), None
patent: 2002236191 (2002-08-01), None
patent: WO99285537 (1999-06-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of stress corrosion cracking mitigation for nuclear... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of stress corrosion cracking mitigation for nuclear..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of stress corrosion cracking mitigation for nuclear... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2724030

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.