ABSTRACT:
The object of this invention is to provide a method for mitigating a stress corrosion cracking of reactor structural material which makes it possible to suppress the rise in the main steam line dose rate without secondary effects such as a rise in the concentration of radioactive cobalt-60, etc. in the reactor water. Hydrogen and a reductive nitrogen compound containing nitrogen having a negative oxidation number (for example, hydrazine) are injected into the core water of boiling water nuclear power plant. By injecting the reductive nitrogen compound containing nitrogen having a negative oxidation number into the core water, the stress corrosion cracking of structural material of reactor can be mitigated without side reactions such as a rise in the concentration of cobalt-60, etc.
REFERENCES:
patent: 3294644 (1966-12-01), Walton
patent: 4376753 (1983-03-01), Lucas
patent: 5084235 (1992-01-01), Ibe et al.
patent: 5135709 (1992-08-01), Andresen et al.
patent: 5164152 (1992-11-01), Kim et al.
patent: 5203984 (1993-04-01), Sakai et al.
patent: 5398268 (1995-03-01), Ibe et al.
patent: 5448605 (1995-09-01), Hettiarachchi
patent: 5600692 (1997-02-01), Hettiarachchi
patent: 6724854 (2004-04-01), Kim et al.
patent: 6793883 (2004-09-01), Andresen et al.
patent: 2002/0080906 (2002-06-01), Andresen et al.
patent: 2002/1118787 (2002-08-01), Andresen et al.
patent: 2003/0012686 (2003-01-01), Andresen et al.
patent: 7209487 (1995-08-01), None
patent: 08327786 (1996-12-01), None
patent: 2766422 (1998-04-01), None
patent: 2001525494 (2001-12-01), None
patent: 2002236191 (2002-08-01), None
patent: 99285537 (1999-06-01), None
Aizawa Motohiro
Endo Masao
Fuse Motomasa
Ishida Kazushige
Nagase Makoto
Brundidge & Stanger, P.C.
Hitachi-GE Nuclear Energy, Ltd.
Palabrica Rick
LandOfFree
Method of stress corrosion cracking mitigating for nuclear... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of stress corrosion cracking mitigating for nuclear..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of stress corrosion cracking mitigating for nuclear... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2651664