ABSTRACT:
Si.sub.3 N.sub.4 ceramics having a glassy phase densification aid are heated while their surface is in contact with SiO.sub.2. The SiO.sub.2 forms one side of a diffusion couple and draws the glassy phase out of the ceramic. The SiO.sub.2 can be provided by heating the ceramic in air to form an SiO.sub.2 scale by the oxidation of Si.sub.3 N.sub.4, or by imbedding the ceramic in SiO.sub.2 powder. Surface pits, if any, formed during oxidation, are removed by grinding.

REFERENCES:
patent: Re28385 (1975-04-01), Mayer
patent: 3411930 (1968-11-01), Reising
patent: 3811928 (1974-05-01), Henney et al.
patent: 3983198 (1976-09-01), Mangels
patent: 4046580 (1977-09-01), Ishii et al.
patent: 4099979 (1978-07-01), Lange et al.
patent: 4102698 (1978-07-01), Lange et al.
patent: 4104442 (1978-08-01), Sussmuth
patent: 4179486 (1979-12-01), Lange

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of strengthening silicon nitride ceramics does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of strengthening silicon nitride ceramics, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of strengthening silicon nitride ceramics will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1630423

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.