ABSTRACT:
Method of straightening a metal bar in which the metal bar is straightened by transporting the metal bar between a pair of rollers at a first straightening pressure. An outer layer portion of the metal bar is then removed in order to provide the metal bar with a reduced diameter and a substantially round cross-section. The metal bar is then again straightened by transporting the metal bar between a pair of rollers at a second straightening pressure. Subsequent to such straightening step, the metal bar desirably is heat treated under stress relieving conditions.
REFERENCES:
patent: 1205998 (1916-11-01), Kenney
patent: 2748038 (1956-04-01), Adair et al.
patent: 3082132 (1963-03-01), Melill et al.
patent: 3094442 (1963-06-01), Perry
patent: 3196052 (1965-07-01), Hann
patent: 3210221 (1965-10-01), Nachtman et al.
patent: 3508978 (1970-04-01), Shuin et al.
patent: 3527078 (1970-09-01), Lawson et al.
patent: 4216666 (1980-08-01), Wu
patent: 4581078 (1986-04-01), Jalil
patent: 4919728 (1990-04-01), Kohl et al.
patent: 5284534 (1994-02-01), Mendes
Slater Steels Corporation
Yee Deborah
LandOfFree
Method of straightening metal bars having extremely low levels o does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of straightening metal bars having extremely low levels o, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of straightening metal bars having extremely low levels o will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2254240