Method of spin-welding

Plastic and nonmetallic article shaping or treating: processes – Including step of generating heat by friction

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

156 735, 264150, 264229, 264248, B29C 4700, B29C 6506

Patent

active

047583924

ABSTRACT:
An end component 3 is spin-welded into the cut end of an extruded tube 1 with the application of axial pressure but without the application of radial pressure to the weld area. The radial forces required to create a weld are provided by hoop stresses which are formed in the tube by shock-cooling the tube as it emerges from the extrusion die. When the tube is cut, the hoop stresses cause the cut end of the tube to contract radially prior to insertion of the end component. To assist in insertion of the end component, a cylindrical skirt thereof 4 is provided with a chamfered end 9.

REFERENCES:
patent: 3120570 (1964-02-01), Kennedy et al.
patent: 3538595 (1970-11-01), Barnes
patent: 3982980 (1976-09-01), Van Manen
patent: 4353761 (1982-10-01), Woerz et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of spin-welding does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of spin-welding, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of spin-welding will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-596291

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.