ABSTRACT:
A solder is disposed outside a joint area without putting a solder foil in an area to be joined or performing preparatory soldering, and soldering is performed by making the melted solder permeate the joint area by a capillary phenomenon. Further, one member is supported by a solder, and a joint solder layer of desired thickness is obtained by use of a jig for supporting the one and the other member at a predetermined distance therebetween when the solder is melted. Further, if a solder outside a joint area is made to stand vertically in its longitudinal direction, and melted at such a state, pressure caused by self-weight is given to the melted solder, and oxide of the solder surface is separated from the melted solder, so that it is possible to further reduce the generation of voids.

REFERENCES:
patent: 3327892 (1967-06-01), Lloyd et al.
patent: 3805373 (1974-04-01), Savolainen et al.
patent: 5172852 (1992-12-01), Bernardoni et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of soldering does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of soldering, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of soldering will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1776178

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.